95430

Sigma-Aldrich

Woods metal

alloy (low melting), granular

Synonim(y):

Tin alloy, nonbase, Bi50 ,Pb25 ,Cd12 ,Sn12 (L-PbBi50Sn12.5Cd12.5), Wood′s alloy

Zaloguj sięWyświetlanie cen organizacyjnych i kontraktowych


About This Item

Numer CAS:
Numer MDL:
Kod UNSPSC:
11101711
Identyfikator substancji w PubChem:
NACRES:
NA.23

Formularz

alloy (low melting)
granular

Poziom jakości

mp

73-77 °C (lit.)
~75 °C

ciąg SMILES

[Cd].[Sn].[Pb].[Bi]

InChI

1S/Bi.Cd.Pb.Sn

Klucz InChI

SSWIVUPIIWJGCS-UHFFFAOYSA-N

Szukasz podobnych produktów? Odwiedź Przewodnik dotyczący porównywania produktów

Powiązane kategorie

Hasło ostrzegawcze

Danger

Zwroty wskazujące rodzaj zagrożenia

Zwroty wskazujące środki ostrożności

Klasyfikacja zagrożeń

Acute Tox. 2 Inhalation - Acute Tox. 4 Oral - Aquatic Acute 1 - Aquatic Chronic 1 - Carc. 1B - Lact. - Muta. 2 - Repr. 1A - STOT RE 1

Organy docelowe

Central nervous system,Blood,Kidney,Immune system

Kod klasy składowania

13 - Non Combustible Solids

Klasa zagrożenia wodnego (WGK)

WGK 3

Temperatura zapłonu (°F)

Not applicable

Temperatura zapłonu (°C)

Not applicable


Wybierz jedną z najnowszych wersji:

Certyfikaty analizy (CoA)

Lot/Batch Number

Nie widzisz odpowiedniej wersji?

Jeśli potrzebujesz konkretnej wersji, możesz wyszukać konkretny certyfikat według numeru partii lub serii.

Masz już ten produkt?

Dokumenty związane z niedawno zakupionymi produktami zostały zamieszczone w Bibliotece dokumentów.

Odwiedź Bibliotekę dokumentów

H Kubo et al.
International journal of radiation oncology, biology, physics, 8(10), 1741-1745 (1982-10-01)
A technique is described to reduce the dose to the contralateral testicle of patients with testis tumors during retroperitoneal therapy with 10 MV X rays. When a conventional clam-shell shielding device was used, the dose to the testis from the
D M Dimitriadis et al.
Medical dosimetry : official journal of the American Association of Medical Dosimetrists, 27(3), 215-220 (2002-10-11)
This study describes the importance of attenuator scatter in the construction of compensators. The attenuator used in this study was Lipowitz metal, commonly referred to as cerrobend. Linear attenuation coefficients of cerrobend were measured in air for different thickness of
Attenuation characteristics of Lipowitz's metal for fast neutrons.
P R Almond et al.
Health physics, 55(1), 91-93 (1988-07-01)
G P Glasgow
Medical dosimetry : official journal of the American Association of Medical Dosimetrists, 16(1), 13-18 (1991-03-01)
Low melting temperature bismuth alloys that contain about 20% to 25% lead and 10% cadmium are widely used in radiotherapy to construct shielding blocks. Since 1980, five papers have addressed questions concerning potential metal toxicity, safe shop practices, measurement of

Produkty

Magnetic materials permeate numerous daily activities in our lives. They are essential components of a diversity of products including hard drives that reliably store information on our computers, decorative magnets that keep the shopping list attached to the refrigerator door, electric bicycles that speed our commute to work, as well as wind turbines for conversion of wind energy to electrical power.

Nasz zespół naukowców ma doświadczenie we wszystkich obszarach badań, w tym w naukach przyrodniczych, materiałoznawstwie, syntezie chemicznej, chromatografii, analityce i wielu innych dziedzinach.

Skontaktuj się z zespołem ds. pomocy technicznej