推薦產品
品質等級
化驗
≥97.0% (NT)
形狀
solid
bp
338-340 °C (lit.)
mp
49-53 °C (lit.)
官能基
amine
hydroxyl
SMILES 字串
Cc1ccc(cc1)N(CCO)CCO
InChI
1S/C11H17NO2/c1-10-2-4-11(5-3-10)12(6-8-13)7-9-14/h2-5,13-14H,6-9H2,1H3
InChI 密鑰
JUVSRZCUMWZBFK-UHFFFAOYSA-N
尋找類似的產品? 前往 產品比較指南
應用
2,2′-(4-Methylphenylimino)diethanol (p-tolyl diethanolamine) was used as an activating amine.
注意
储存时可能变为棕色
訊號詞
Danger
危險分類
Acute Tox. 4 Oral - Aquatic Chronic 3 - Eye Dam. 1 - Skin Sens. 1
儲存類別代碼
11 - Combustible Solids
水污染物質分類(WGK)
WGK 3
閃點(°F)
Not applicable
閃點(°C)
Not applicable
個人防護裝備
dust mask type N95 (US), Eyeshields, Gloves
客戶也查看了
M P Patel et al.
Biomaterials, 12(7), 649-652 (1991-09-01)
A number of useful room temperature polymerizing resins were formulated, based on poly(ethyl methacrylate) powder and a range of low shrinkage heterocyclic methacrylate monomers. N,N-dimethyl-p-toluidine or p-tolyl diethanolamine were used as activating amines, but the latter material is less active
G J Pomrink et al.
Biomaterials, 24(6), 1023-1031 (2002-12-31)
The primary objective of this research is to evaluate the reaction kinetics of CORTOSS(TM), a thermoset, Bis-GMA (2,2-bis[4-(2-hydroxymethacryloxypropyl) phenyl]propane) composite system as a function of time, material storage temperature and the temperature of the surrounding environment (site temperature). This study
K Ikemura et al.
Dental materials journal, 15(2), 132-143 (1996-12-01)
To develop a self-etching primer for ground dentin, 4-acryloxyethyltrimellitic acid (4-AET) was newly synthesized, and the effect of concentrations varying from 0 (control) to 56.5 wt% 4-AET in the water/ HEMA primer on bonding to the dentin was investigated. Bond
Ulrich Salz et al.
The journal of adhesive dentistry, 7(1), 7-17 (2005-05-17)
To investigate the influence of the acid-base reaction between acidic monomers and amines on the polymerization behavior of self-etching, self-curing adhesives, determine the effect of the application mode on the shear bond strength and morphology, and elucidate the adhesion performance
H H Xu et al.
Journal of biomedical materials research, 52(4), 812-818 (2000-10-18)
The strength and toughness of dental core buildup composites in large stress-bearing restorations need to be improved to reduce the incidence of fracture due to stresses from chewing and clenching. The aims of the present study were to develop novel