추천 제품
Grade
technical grade
Quality Level
형태
liquid
불순물
<25% polymer
refractive index
n20/D 1.457 (lit.)
bp
226-229 °C (lit.)
58-60 °C/0.5 mmHg (lit.)
mp
−13-−12 °C (lit.)
density
1.079 g/mL at 25 °C (lit.)
저장 온도
−20°C
SMILES string
O=C1CCCCO1
InChI
1S/C5H8O2/c6-5-3-1-2-4-7-5/h1-4H2
InChI key
OZJPLYNZGCXSJM-UHFFFAOYSA-N
유사한 제품을 찾으십니까? 방문 제품 비교 안내
애플리케이션
δ-Valerolactone (tetrahydro-2H-2-pyranone or δ VL) can be used as a monomer unit in the synthesis of poly(δ-valerolactone)s poly(conjugated ester)s via ring-opening polymerization.
It can also be used as a starting material in the synthesis of (+)-guadinomic acid , sodium δ-hydroxyvalerate , methyl δ-hydroxyvalerate , and 5-hydroxyvaleraldehyde.
It can also be used as a starting material in the synthesis of (+)-guadinomic acid , sodium δ-hydroxyvalerate , methyl δ-hydroxyvalerate , and 5-hydroxyvaleraldehyde.
신호어
Danger
유해 및 위험 성명서
예방조치 성명서
Hazard Classifications
Eye Dam. 1
Storage Class Code
10 - Combustible liquids
WGK
WGK 1
Flash Point (°F)
233.6 °F - closed cup
Flash Point (°C)
112 °C - closed cup
개인 보호 장비
Eyeshields, Gloves, type ABEK (EN14387) respirator filter
이미 열람한 고객
Organic letters, 14(9), 2410-2413 (2012-04-26)
A palladium-catalyzed decarboxylative cyclopropanation of γ-methylidene-δ-valerolactones with aromatic aldehydes has been developed to give 4-oxaspiro[2.4]heptanes with high selectivity. The site of nucleophilic attack to a π-allylpalladium intermediate has been controlled with a sterically demanding phosphine ligand. The course of the
Diphenyl phosphate as an efficient cationic organocatalyst for controlled/living ring-opening polymerization of δ-valerolactone and ε-caprolactone
Macromolecules, 44(7), 1999-2005 (2011)
The Journal of organic chemistry, 73(7), 2674-2678 (2008-03-08)
gamma-Butyrolactone, unlike delta-valerolactone, does not polymerize despite a strain energy of approximately 8 kcal mol-1 which could be relieved by opening the s-cis lactone ester bond to an s-trans ester bond in the polymer. To explain this anomaly, we have
Organolanthanide-initiated living polymerizations of ε -caprolactone, δ-valerolactone, and β-propiolactone
Macromolecules, 29(5), 1798-1806 (1996)
Biomacromolecules, 12(9), 3265-3274 (2011-07-16)
Biodegradable polyurethane urea (PUU) elastomers are ideal candidates for fabricating tissue engineering scaffolds with mechanical properties akin to strong and resilient soft tissues. PUU with a crystalline poly(ε-caprolactone) (PCL) macrodiol soft segment (SS) showed good elasticity and resilience at small
자사의 과학자팀은 생명 과학, 재료 과학, 화학 합성, 크로마토그래피, 분석 및 기타 많은 영역을 포함한 모든 과학 분야에 경험이 있습니다..
고객지원팀으로 연락바랍니다.