酸化亜鉛ナノ粒子インク

2.5 wt. %, viscosity 10 cP, work function -4.3eV

別名:

Avantama N-10-Jet, Nanograde N-10-Jet, ZnO ink, ZnO nanoparticle ink, zinc oxide dispersion, zinc oxide suspension

ログイン組織・契約価格を表示する


About This Item

UNSPSCコード:
12352103
NACRES:
NA.23

品質水準

形状

dispersion

濃度

2.5 wt. % (crystalline ZnO in isopropanol and propylene glycol)

仕事関数

-4.1--4.5 eV

translucent brownish

粒径

8-16 nm

粘度

8-14 cP

類似した製品をお探しですか? 訪問 製品比較ガイド

アプリケーション

ZnO nanoparticle ink is for inkjet printing for the use as electron transport layer in printed electronics. ZnO nanoparticle ink is universally applicable in normal and inverted architecture.

調製ノート

  • Storage: In dark at room temperature.
  • Prior to application: Shake, ultrasonicate with sonic horn and (optionally) filter through 0.45μm PTFE filter.
  • Post-treatment: Annealing of deposited ZnO films at >120°C.

法的情報

Product of Avantama Ltd.

ピクトグラム

FlameExclamation markEnvironment

シグナルワード

Danger

危険有害性情報

危険有害性の分類

Aquatic Chronic 2 - Eye Irrit. 2 - Flam. Liq. 2 - STOT SE 3

ターゲットの組織

Central nervous system

保管分類コード

3 - Flammable liquids

WGK

WGK 2

引火点(°F)

71.6 °F

引火点(℃)

22 °C


適用法令

試験研究用途を考慮した関連法令を主に挙げております。化学物質以外については、一部の情報のみ提供しています。 製品を安全かつ合法的に使用することは、使用者の義務です。最新情報により修正される場合があります。WEBの反映には時間を要することがあるため、適宜SDSをご参照ください。

消防法

第4類:引火性液体
第二石油類
危険等級III
非水溶性液体

労働安全衛生法名称等を表示すべき危険物及び有害物

名称等を表示すべき危険物及び有害物

労働安全衛生法名称等を通知すべき危険物及び有害物

名称等を通知すべき危険物及び有害物

Jan Code

807613-VAR:
807613-50ML:4548173347820
807613-5ML:4548174013144
807613-BULK:
807613-10ML:4548173347813


試験成績書(COA)

製品のロット番号・バッチ番号を入力して、試験成績書(COA) を検索できます。ロット番号・バッチ番号は、製品ラベルに「Lot」または「Batch」に続いて記載されています。

以前この製品を購入いただいたことがある場合

文書ライブラリで、最近購入した製品の文書を検索できます。

文書ライブラリにアクセスする

R P Warrell et al.
Annals of internal medicine, 113(11), 847-851 (1990-12-01)
To evaluate whether a brief course of treatment with gallium nitrate can reduce biochemical parameters of accelerated bone turnover in patients with advanced Paget disease. Unblinded trial, decreasing dose schedules of gallium nitrate. University hospital with primary orthopedic and metabolic
Mohammad Vaseem et al.
Journal of nanoscience and nanotechnology, 12(3), 2380-2386 (2012-07-05)
Zinc oxide (ZnO) nanoparticles were synthesized by ultrasonically-assisted solution process without using any surfactants. The as-synthesized spherical ZnO nanoparticles with diameter of 20 +/- 5 nm possessed crystalline nature with wurtzite hexagonal phase and showed a blue-shifted near band-edge ultra-violet

資料

Professor Tokito and Professor Takeda share their new materials, device architecture design principles, and performance optimization protocols for printed and solution-processed, low-cost, highly flexible, organic electronic devices.

Recent progress in the area of solution-processed functional materials has led to the development of a variety of thin-film optoelectronic devices with significant promise in the industrial and consumer electronics fields.

Recent progress in the area of solution-processed functional materials has led to the development of a variety of thin-film optoelectronic devices with significant promise in the industrial and consumer electronics fields.

ライフサイエンス、有機合成、材料科学、クロマトグラフィー、分析など、あらゆる分野の研究に経験のあるメンバーがおります。.

製品に関するお問い合わせはこちら(テクニカルサービス)