跳转至内容
Merck

345326

Sigma-Aldrich

聚(四氢呋喃)

average Mn ~2,000, contains BHT as stabilizer

别名:

Terathane®2000 聚醚二元醇, α-氢-ω-羟基聚(氧-1,4-丁二基), 聚(1,4-丁二醇), 聚THF

登录查看公司和协议定价


About This Item

线性分子式:
H(OCH2CH2CH2CH2)nOH
CAS号:
MDL號碼:
分類程式碼代碼:
12162002
PubChem物質ID:
NACRES:
NA.23

蒸汽壓力

<0.01 mmHg ( 25 °C)
<1 mmHg ( 20 °C)

形狀

solid

分子量

average Mn ~2,000

包含

BHT as stabilizer

mp

28-40 °C

密度

0.972 g/mL at 25 °C

SMILES 字串

OCCCCO

InChI

1S/C8H18O2/c1-3-5-6-10-8(4-2)7-9/h8-9H,3-7H2,1-2H3/t8-/m0/s1

InChI 密鑰

BJZYYSAMLOBSDY-QMMMGPOBSA-N

正在寻找类似产品? 访问 产品对比指南

應用

聚四氢呋喃(PTHF) 可作为大分子引发剂用于通过开环聚合反应制备嵌段共聚物 。

交联PTHF可作为 基质用于制备锂离子电池中的热稳定聚合物电解质 。

它还可作为起始原料用于合成药物和基因递送的环糊精基超分子络合物。

法律資訊

DuPont 产品
Terathane is a registered trademark of Invista North America S.a.r.l.

危險聲明

防範說明

危險分類

Aquatic Chronic 3

儲存類別代碼

10 - Combustible liquids

水污染物質分類(WGK)

WGK 3

個人防護裝備

dust mask type N95 (US), Eyeshields, Gloves


历史批次信息供参考:

分析证书(COA)

Lot/Batch Number

没有发现合适的版本?

如果您需要特殊版本,可通过批号或批次号查找具体证书。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

其他客户在看

M Renier et al.
Journal of biomaterials science. Polymer edition, 5(3), 231-244 (1993-01-01)
Poly(etherurethane urea) (PEUU) elastomers when employed as biomedical devices may be susceptible to extraction upon implantation. Four PEUU elastomers containing a single PEUU formulation, but varying in terms of their additives, were subjected to an in vitro extraction procedure. The
P Banu et al.
Journal of colloid and interface science, 277(2), 304-308 (2004-09-03)
Aqueous dispersions of poly(ester-imide)s [P(E-I)s] have been prepared by dispersing the P(E-I)s in water without any external solubilizing agents. P(E-I)s were prepared from anhydride-terminated polyester prepolymer and diisocyanate. The -COOH groups in the polymer were then neutralized using triethylamine and
Antony Memboeuf et al.
Journal of the American Society for Mass Spectrometry, 22(10), 1744-1752 (2011-09-29)
Collision induced dissociation tandem mass spectrometry experiments were performed to unequivocally separate compounds from an isobaric mixture of two products. The Survival Yield curve was obtained and is shown to consist in a linear combination of the curves corresponding to
W K Loke et al.
Biomaterials, 17(22), 2163-2172 (1996-11-01)
Hybrid biomaterials have been produced by the interaction of polyurethane oligomers with both fresh and glutaraldehyde-fixed porcine pericardium. The hybrid biomaterials so formed were translucent with occasional white streaks and/or spots, had increased stiffness (to touch) but remained pliable. No
R S Labow et al.
Journal of biomaterials science. Polymer edition, 8(10), 779-795 (1997-01-01)
Although biodegradation of model poly(ester-urethane)s and poly(ether-urethane)s has been demonstrated using a single enzyme system (cholesterol esterase (CE) in vitro, in vivo biodegradation most likely involves many processes acting together. In this study, the physical (film vs textured surface) and