GF37671228

Tantalum

foil, light tested, 150x150mm, thickness 0.034mm, as rolled, 99.9%

Sinonimo/i:

Tantalum, TA000347, Ta

Autenticatiper visualizzare i prezzi riservati alla tua organizzazione & contrattuali


About This Item

Formula empirica (notazione di Hill):
Ta
Numero CAS:
Peso molecolare:
180.95
Numero MDL:
Codice UNSPSC:
12352300
ID PubChem:
NACRES:
NA.23

Tensione di vapore

<0.01 mmHg ( 537.2 °C)

Saggio

99.9%

Forma fisica

foil

Temp. autoaccensione

572 °F

Produttore/marchio commerciale

Goodfellow 376-712-28

Resistività

13.5 μΩ-cm, 20°C

Misura × spessore

150x150 mm × 0.034 mm

P. eboll.

5425 °C (lit.)

Punto di fusione

2996 °C (lit.)

Densità

16.69 g/cm3 (lit.)

Stringa SMILE

[Ta]

InChI

1S/Ta
GUVRBAGPIYLISA-UHFFFAOYSA-N

Descrizione generale

For updated SDS information please visit www.goodfellow.com.

Note legali

Product of Goodfellow

Certificati d'analisi (COA)

Cerca il Certificati d'analisi (COA) digitando il numero di lotto/batch corrispondente. I numeri di lotto o di batch sono stampati sull'etichetta dei prodotti dopo la parola ‘Lotto’ o ‘Batch’.

Possiedi già questo prodotto?

I documenti relativi ai prodotti acquistati recentemente sono disponibili nell’Archivio dei documenti.

Visita l’Archivio dei documenti

Yingxun Du et al.
Journal of hazardous materials, 225-226, 21-27 (2012-05-23)
In order to overcome the limitation of the application of nanoparticles, tantalum (oxy)nitrides nanotube arrays on a Ta foil were synthesized and introduced in vis (visible light)-Fenton-like system to enhance the degradation of atrazine. At first, the anodization of tantalum
Zhongli Cai et al.
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
J G Sen Gupta
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
Zhongli Cai et al.
Radiation research, 165(3), 365-371 (2006-02-24)
Both thick and thin films of pGEMR-3Zf- plasmid DNA deposited on a tantalum foil were exposed to soft X rays (effective energy of 14.8 keV) for various times in air under a relative humidity of 45% (Gamma approximately 6, where
J G Sen Gupta
Talanta, 32(1), 1-6 (1985-01-01)
An improved graphite furnace atomic-absorption method has been developed for the determination of Sc, Y and the rare-earth elements in silicate rocks and related materials. The method, which involves the separation of the lanthanides by ion-exchange followed by their determination

Il team dei nostri ricercatori vanta grande esperienza in tutte le aree della ricerca quali Life Science, scienza dei materiali, sintesi chimica, cromatografia, discipline analitiche, ecc..

Contatta l'Assistenza Tecnica.