30620

Sigma-Aldrich

氢氧化钠

puriss. p.a., ACS reagent, reag. Ph. Eur., K ≤0.02%, ≥98%, pellets

同義詞:

‘苛性钠’

登入查看組織和合約定價


About This Item

線性公式:
NaOH
CAS號碼:
分子量::
40.00
EC號碼:
MDL號碼:
分類程式碼代碼:
12352302
PubChem物質ID:
NACRES:
NA.21

等級

ACS reagent
puriss. p.a.

品質等級

agency

reag. Ph. Eur.

蒸汽密度

>1 (vs air)

蒸汽壓力

<18 mmHg ( 20 °C)
3 mmHg ( 37 °C)

化驗

≥98%

形狀

pellets

技術

titration: suitable

雜質

≤0.0003% total nitrogen (N)
≤0.0005% heavy metals (as Pb)
≤1% Na2CO3

mp

318 °C (lit.)

溶解度

water: soluble 1260 g/L at 20 °C

密度

2.13 g/cm3 at 20 °C

負離子痕跡

chloride (Cl-): ≤10 mg/kg
phosphate (PO43-): ≤5 mg/kg
silicate (as SiO2): ≤10 mg/kg
sulfate (SO42-): ≤30 mg/kg

正離子痕跡

Al: ≤5 mg/kg
As: ≤1 mg/kg
Ca: ≤5 mg/kg
Cu: ≤5 mg/kg
Fe: ≤5 mg/kg
Hg: ≤0.05 mg/kg
K: ≤200 mg/kg
Mg: ≤5 mg/kg
Ni: ≤5 mg/kg
Pb: ≤2 mg/kg
Zn: ≤5 mg/kg

儲存溫度

15-25°C

SMILES 字串

[OH-].[Na+]

InChI

1S/Na.H2O/h;1H2/q+1;/p-1

InChI 密鑰

HEMHJVSKTPXQMS-UHFFFAOYSA-M

尋找類似的產品? 前往 產品比較指南

一般說明

氢氧化钠是无机碱。它参与由 Au/木炭或 Au/石墨催化的甘油氧化。它还参与无溶剂羟醛缩合反应。

應用

氢氧化钠可用于通过滴定测定胶体二氧化硅的比表面积。它可用于硼氢化钠的直接氧化,其通过循环和线性伏安法、计时电流法和计时电位法进行研究。它可用于组成柠檬酸盐缓冲液和硼酸盐缓冲液。
它可用于以下化合物的合成:
  • 烷基芳基氨基磺基甜菜碱
  • 3-[4-辛基苯氧基乙氧基乙氧基乙基]二甲基氨基丙磺酸盐(XOSB)
  • 三磺基甜菜碱(TriSBn)

象形圖

Corrosion

訊號詞

Danger

危險聲明

危險分類

Eye Dam. 1 - Met. Corr. 1 - Skin Corr. 1A

儲存類別代碼

8A - Combustible corrosive hazardous materials

水污染物質分類(WGK)

WGK 1

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析證明 (COA)

輸入產品批次/批號來搜索 分析證明 (COA)。在產品’s標籤上找到批次和批號,寫有 ‘Lot’或‘Batch’.。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

客戶也查看了

M A Roberts et al.
Analytical chemistry, 69(11), 2035-2042 (1997-06-01)
This report describes a UV laser photoablation method for the production of miniaturized liquid-handling systems on polymer substrate chips. The fabrication of fluid channel and reservoir networks is accomplished by firing 200 mJ pulses from an UV excimer laser at
Chemoselective, solvent-free aldol condensation reaction.
Raston CL and Scott JL.
Green Chemistry, 2(2), 49-52 (2000)
M Chevallet et al.
Electrophoresis, 19(11), 1901-1909 (1998-09-18)
Severe quantitative loss of protein is often observed in high-resolution two-dimensional electrophoresis of membrane proteins, while the resolution is usually not affected. To improve the solubility of proteins in this technique, we tested denaturing cocktails containing various detergents and chaotropes.
Kinetics of sodium borohydride direct oxidation and oxygen reduction in sodium hydroxide electrolyte: Part I. BH4- electro-oxidation on Au and Ag catalysts.
Chatenet M, et al.
Electrochimica Acta, 51(25), 5459-5467 (2006)
Silvio Carrettin et al.
Chemical communications (Cambridge, England), (7)(7), 696-697 (2002-07-18)
Glycerol is oxidised to glyceric acid with 100% selectivity using either 1% Au/charcoal or 1% Au/graphite catalyst under mild reaction conditions (60 degrees C, 3 h, water as solvent).

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務