跳轉至內容
Merck
全部照片(3)

重要文件

544760

Sigma-Aldrich

氧化锆(IV)

nanopowder, <100 nm particle size (TEM)

同義詞:

二氧化锆

登入查看組織和合約定價


About This Item

線性公式:
ZrO2
CAS號碼:
分子量::
123.22
EC號碼:
MDL號碼:
分類程式碼代碼:
12352302
PubChem物質ID:
NACRES:
NA.23

形狀

nanopowder

反應適用性

reagent type: catalyst
core: zirconium

表面積

≥25 m2/g

粒徑

<100 nm (TEM)

bp

5000 °C (lit.)

mp

2700 °C (lit.)

密度

5.89 g/mL at 25 °C (lit.)

SMILES 字串

O=[Zr]=O

InChI

1S/2O.Zr

InChI 密鑰

MCMNRKCIXSYSNV-UHFFFAOYSA-N

尋找類似的產品? 前往 產品比較指南

一般說明

二氧化锆(IV)(ZrO2) ,也称为氧化锆,是陶瓷纳米颗粒,可用作纳米填料。 可将其掺入各种聚合物和金属复合材料中,改善基础材料的热机械性能。

應用

ZrO2 可用作PMMA上的填充材料,进一步作为高强度的义齿基础材料。 也可用作基于复合材料的金属涂层,改善基础材料的整体机械性能。

儲存類別代碼

11 - Combustible Solids

水污染物質分類(WGK)

nwg

閃點(°F)

Not applicable

閃點(°C)

Not applicable

個人防護裝備

dust mask type N95 (US), Eyeshields, Gloves


從最近期的版本中選擇一個:

分析證明 (COA)

Lot/Batch Number

未看到正確版本?

如果您需要一個特定的版本,您可以透過批號來尋找特定憑證。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

客戶也查看了

Slide 1 of 1

1 of 1

Friction and wear behavior of zirconium oxide reinforced PMMA composites
Akinci A, et al.
Composites Part B: Engineering, 56(1-2), 42-47 (2014)
Support and solvent effects on the liquid-phase chemoselective hydrogenation of crotonaldehyde over Pt catalysts
Hidalgo-Carrillo J, et al.
Applied Catalysis A: General, 385(1-2), 190-200 (2010)
Paolo Vigolo et al.
Journal of prosthodontics : official journal of the American College of Prosthodontists, 17(8), 621-626 (2008-09-19)
The purpose of this study was to assess in vitro the marginal fit of four-unit fixed partial dentures (FPDs) produced using three different computer aided design/computer aided manufacturing (CAD/CAM) all-ceramic systems before and after porcelain firing cycles and after glaze
Zhongpu Zhang et al.
Acta biomaterialia, 9(9), 8394-8402 (2013-05-21)
Effective and reliable clinical uses of dental ceramics necessitate an insightful analysis of the fracture behaviour under critical conditions. To better understand failure characteristics of porcelain veneered to zirconia core ceramic structures, thermally induced cracking during the cooling phase of
Katarzyna Zielińska et al.
Journal of colloid and interface science, 377(1), 362-367 (2012-04-14)
Ni-P-nano-ZrO(2) coatings were produced using the electroless deposition technique. To prevent agglomeration of zirconia nanoparticles in the plating bath, various surfactant additives (anionic, cationic, and nonionic) were used. The most stable bath was obtained with the addition of dodecyltrimethylammonium bromide

文章

Hydrogen is one of the most important resources in providing food, fuel, and chemical products for our everyday life. Sustainable catalytic hydrogen production from bioethanol has gained significant attention in recent years due to globally diminishing fossil fuel supplies, which have necessitated the search for new chemical feedstocks.

A key challenge for nanomaterial safety assessment is the ability to handle the large number of newly engineered nanomaterials (ENMs), including developing cost-effective methods that can be used for hazard screening.

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務