双酚 A 甘油二丙烯酸

contains MEHQ as inhibitor

同義詞:

2,2-双[4-(3-丙烯酰氧基-2-羟基丙氧基)苯基]丙烷, 2,2-双[丙烯酰氧基(2′-羟丙氧基)苯基]丙烷, 双酚 A 甘油醇酸二丙烯酸酯

登入查看組織和合約定價


About This Item

經驗公式(希爾表示法):
C27H32O8
CAS號碼:
分子量::
484.54
EC號碼:
MDL號碼:
分類程式碼代碼:
12162002
PubChem物質ID:
NACRES:
NA.23

包含

MEHQ as inhibitor
250-500 ppm MEHQ as inhibitor

折射率

n20/D 1.557 (lit.)

黏度

2000-4000 cP(65 °C)(lit.)

酸值

<5 mg KOH/g

密度

1.18 g/mL at 25 °C (lit.)

SMILES 字串

CC(C)(c1ccc(OCC(O)COC(=O)C=C)cc1)c2ccc(OCC(O)COC(=O)C=C)cc2

InChI

1S/C27H32O8/c1-5-25(30)34-17-21(28)15-32-23-11-7-19(8-12-23)27(3,4)20-9-13-24(14-10-20)33-16-22(29)18-35-26(31)6-2/h5-14,21-22,28-29H,1-2,15-18H2,3-4H3

InChI 密鑰

VZTQQYMRXDUHDO-UHFFFAOYSA-N

應用

紫外光固化交联试剂。可固化油墨、涂料、清漆和腊克漆的组分。

特點和優勢

高粘度、非挥发性、双官能化丙烯酸酯。固化速度快、气味小、挥发性低。

外觀

环氧丙烯酸酯低聚物

象形圖

Exclamation mark

訊號詞

Warning

危險聲明

危險分類

Skin Sens. 1

儲存類別代碼

10 - Combustible liquids

水污染物質分類(WGK)

WGK 3

閃點(°F)

235.4 °F - closed cup

閃點(°C)

113 °C - closed cup

個人防護裝備

Eyeshields, Faceshields, Gloves, type ABEK (EN14387) respirator filter


從最近期的版本中選擇一個:

分析證明 (COA)

Lot/Batch Number

未看到正確版本?

如果您需要一個特定的版本,您可以透過批號來尋找特定憑證。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

D L Holness et al.
Contact dermatitis, 28(4), 216-219 (1993-04-01)
Epoxy resin of the bisphenol A type (ERBA) is a common cause of occupational contact dermatitis. 167 patients with a history of potential exposure were patch tested with epoxy resin (molecular weight 340) (ERBAM) 1% in pet. and with a
Occupational allergic contact dermatitis from 2,2-bis[4-(2-hydroxy-3-acryloxypropoxy)phenyl]-propane (epoxy diacrylate) in ultraviolet-cured inks.
L Kanerva et al.
Contact dermatitis, 43(1), 56-59 (2000-07-21)
B Björkner
Acta dermato-venereologica, 61(1), 7-10 (1981-01-01)
One commonly used prepolymer in ultraviolet (UV) curing inks is epoxy acrylate. Of 6 men with dermatitis contracted from UV-curing inks, 2 had positive patch test reaction to epoxy acrylate. None reacted to the chemically related bisphenol A dimethacrylate. The
M Bruze et al.
Dermatosen in Beruf und Umwelt. Occupation and environment, 37(5), 171-176 (1989-09-01)
In December, 1985, and February, 1986, skin diseases were investigated among workers in a plant producing printed circuit boards made of copper sheets and fiberglass fabric impregnated with a brominated epoxy resin. A questionnaire was sent to all 159 employees
Shaoxia Yang et al.
Journal of hazardous materials, 178(1-3), 786-791 (2010-03-09)
Epoxy acrylate monomer industrial wastewater contained highly concentrated and toxic organic compounds. The wet air oxidation (WAO) and catalytic wet air oxidation (CWAO) were used to eliminate pollutants in order to examine the feasibility of the WAO/CWAO as a pre-treatment

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務