추천 제품
Agency
reag. ISO
reag. Ph. Eur.
Quality Level
vapor pressure
1 mmHg ( 745 °C)
제품 라인
EMSURE®
분석
≥99.5% (silver nitrate titration)
99.5-100.5% dry basis (silver nitrate titration)
형태
solid
효능
2779 mg/kg LD50, oral (Rat)
불순물
≤0.001% Total nitrogen (N)
손실
≤0.1% loss on drying, 105 °C
pH
6.9 (20 °C, 50 g/L in H2O)
bp
1325 °C/1013 hPa
mp
681 °C (lit.)
solubility
1430 g/L
벌크 밀도
1500 kg/m3
음이온 미량물
chloride, bromide (as Cl)-: ≤0.01%
iodate (IO3-): ≤0.0003%
phosphate (PO43-): ≤0.001%
sulfate (SO42-): ≤0.001%
thiosulfate (S2O32-): passes test
양이온 미량물
As: ≤0.00001%
Ba: ≤0.002%
Ca: ≤0.001%
Cu: ≤0.0002%
Fe: ≤0.0002%
Mg: ≤0.001%
N: ≤0.001%
Na: ≤0.03%
Pb: ≤0.0002%
heavy metals (as Pb): ≤0.0005%
저장 온도
2-30°C
SMILES string
[K+].[I-]
InChI
1S/HI.K/h1H;/q;+1/p-1
InChI key
NLKNQRATVPKPDG-UHFFFAOYSA-M
유사한 제품을 찾으십니까? 방문 제품 비교 안내
관련 카테고리
애플리케이션
- Influence of silver fluoride plus potassium iodine on adhesive properties of primary carious dentin-resin interface: An in vitro study.: This study examines how potassium iodide, in combination with silver fluoride, impacts the bonding properties of dental resin to carious dentin, highlighting its potential in dental treatments (da Luz et al., 2024).
- Comparisons of ammonia- and water-based silver-containing solutions on dentin bonding and enzymatic activity: 1-yr evaluation.: The research investigates the effects of potassium iodide in silver-containing solutions on dentin bonding and enzyme activity, providing insights into dental material performance over time (D′ Alessandro et al., 2024).
- Multi-spectroscopic and in silico investigation of gambogic acid-calf thymus DNA interactions.: This study utilizes potassium iodide in spectroscopic methods to elucidate the interactions between gambogic acid and DNA, contributing to the understanding of its potential therapeutic effects (Bhardwaj et al., 2024).
- Surface Modification of Lignite with Alkyl and Mixed Alkyl-Aryl Films Generated from an Aryl Diazonium Salt and Alkyl Halides: Experimental Results and Theoretical Analyses.: Research details the use of potassium iodide in the surface modification of lignite, presenting a blend of experimental and theoretical insights to improve material properties (Hasani et al., 2024).
분석 메모
Assay (argentometric; calculated on dried substance): 99.5 - 100.5 %
Identity: passes test
Appearance of solution: passes test
Alkaline impurities: passes test
pH-value (5 %; water): 6 - 8
Chloride and Bromide (as Cl): ≤ 0.01 %
Iodate (IO₃): ≤ 0.0003 %
Phosphate (PO₄): ≤ 0.001 %
Sulfate (SO₄): ≤ 0.001 %
Thiosulfate (S₂O₃): passes test
Total nitrogen (N): ≤ 0.001 %
Heavy metals (as Pb): ≤ 0.0005 %
As (Arsenic): ≤ 0.00001 %
Ba (Barium): ≤ 0.002 %
Ca (Calcium): ≤ 0.001 %
Cu (Copper): ≤ 0.0002 %
Fe (Iron): ≤ 0.0002 %
Mg (Magnesium): ≤ 0.001 %
Na (Sodium): ≤ 0.03 %
Pb (Lead): ≤ 0.0002 %
Reducing substances: passes test
Loss on Drying (105 °C): ≤ 0.1 %
법적 정보
신호어
Danger
유해 및 위험 성명서
예방조치 성명서
Hazard Classifications
STOT RE 1 Oral
표적 기관
Thyroid
Storage Class Code
6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects
WGK
WGK 3
Flash Point (°F)
Not applicable
Flash Point (°C)
Not applicable
시험 성적서(COA)
제품의 로트/배치 번호를 입력하여 시험 성적서(COA)을 검색하십시오. 로트 및 배치 번호는 제품 라벨에 있는 ‘로트’ 또는 ‘배치’라는 용어 뒤에서 찾을 수 있습니다.
이미 열람한 고객
프로토콜
Preparation of a standard solution for Chlorine dioxide acc. to DIN EN ISO 7393
Preparation of a standard solution for Monochloramine.
AQA Standard for free chlorine - Preparation of a standard solution for free chlorine
자사의 과학자팀은 생명 과학, 재료 과학, 화학 합성, 크로마토그래피, 분석 및 기타 많은 영역을 포함한 모든 과학 분야에 경험이 있습니다..