추천 제품
vapor pressure
0.02 mmHg ( 100 °C)
분석
≥90%
형태
liquid
포함
75.0-125.0 hydroquinone as inhibitor
refractive index
n20/D 1.458 (lit.)
bp
>315 °C (lit.)
density
0.995 g/mL at 25 °C (lit.)
SMILES string
CC(=C)C(=O)OCCCCCCOC(=O)C(C)=C
InChI
1S/C14H22O4/c1-11(2)13(15)17-9-7-5-6-8-10-18-14(16)12(3)4/h1,3,5-10H2,2,4H3
InChI key
SAPGBCWOQLHKKZ-UHFFFAOYSA-N
유사한 제품을 찾으십니까? 방문 제품 비교 안내
신호어
Warning
유해 및 위험 성명서
Hazard Classifications
Eye Irrit. 2 - Skin Irrit. 2 - STOT SE 3
표적 기관
Respiratory system
Storage Class Code
10 - Combustible liquids
WGK
WGK 2
Flash Point (°F)
228.2 °F - closed cup
Flash Point (°C)
109 °C - closed cup
개인 보호 장비
Eyeshields, Gloves, type ABEK (EN14387) respirator filter
시험 성적서(COA)
제품의 로트/배치 번호를 입력하여 시험 성적서(COA)을 검색하십시오. 로트 및 배치 번호는 제품 라벨에 있는 ‘로트’ 또는 ‘배치’라는 용어 뒤에서 찾을 수 있습니다.
이미 열람한 고객
Dental materials : official publication of the Academy of Dental Materials, 14(6), 385-393 (1999-09-14)
To explore possible enhancement of the mechanical properties of resin composites by aligning the filler particles. The resin for the composites consisted of urethane dimethacrylate (UDMA) and 1,6-hexanediol dimethacrylate (HDDMA) mixed in the ratio of 90 to 10; the filler
Journal of oral rehabilitation, 28(2), 180-185 (2001-04-12)
The purpose of this study was to clarify the effect of the reducing agent on the oxygen-inhibited layer of the cross-linked reline material. A commercial autopolymerizing reline resin containing 1,6-hexanediol dimethacrylate as cross-linking agent and 1 wt.% sodium sulphite solution
Journal of oral rehabilitation, 22(3), 183-189 (1995-03-01)
The effect of silanation on the dispersion of quartz and zirconia-silica fillers by monomers used to formulate composites was studied. Sixteen silane coupling agents and three methods were used, and the amounts of the monomers needed to reach wet and
Primary dental care : journal of the Faculty of General Dental Practitioners (UK), 8(4), 151-155 (2002-01-22)
The fit of the denture base to the alveolar ridge progressively declines with alveolar ridge resorption. Once a denture becomes ill-fitting there are two main treatment options: to construct a new denture or to restore the fit of the existing
Dental materials : official publication of the Academy of Dental Materials, 27(8), 818-824 (2011-05-21)
A great challenge regarding the ease-of-use of composites involves the development of 'self-adhesive' composites that no longer require a separate adhesive to bond to tooth enamel/dentin. To characterize the interfacial ultra-structure of an experimental self-adhesive filling material bonded to enamel