推荐产品
帶隙
3.57 eV, Optical, Solution state
品質等級
溶解度
soluble (THF > 1 mg /mL, MeCN < 0.33 mg / mL, DMSO < 0.03 mg / mL, DCM > 1 mg /mL)
λmax
164,000 M-1cm-1 at 272 nm in ethyl acetate
螢光
λem 494 nm, quantum yield 0.55 (pSS (nm) = 222, Fluorescence Lifetime (ns) = 5.45)
軌道能量
HOMO -5.45 eV (CV)
LUMO -2.47 eV (CV)
儲存溫度
−20°C
一般說明
- Thermal degradation onset = ∼380 °C
- Polymorph crystalline phase: Solid, Discotic Liquid Crystal, Isotropic
- Phase transition temperature:
- Heating: Crys - Colh – 96 °C, Colh - Iso – 168 °C
- Cooling: Iso - Colh – 161 °C, Colh - Crys – 43 °C
TpOx-2-Nap is a UV excitable fluorescent material with a polycyclic aromatic donor-acceptor structure where the triphenoxazole core acts as a donor and the aromatic group on the two position of the oxazole (2-naphthalene) act as the acceptor group. The push-pull, donor-acceptor, structure facilitates intramolecular charge transfer in the excited state that results in a 222 nm emission Stokes Shift. This oxazole is also a photo-conducting Discotic Liquid Crystalline (DLC) material with mesophase transition onset temperature of 96 °C. It is designed for 355 nm and 405 nm excitation with emission at 494 nm with quantum yield of 0.55, high thermal, chemical and photostability. This luminescent compound has potential uses in fluorescent dye staining, organic electronic and photonics, and imaging applications.
應用
Fluorescent materials have a range of unique properties that allows for potential use in a range of applications:
- Fluorescent dye staining
- Organic semiconductor for organic electronic and photonic applications
- Multi-photon microscopy
儲存和穩定性
Store under nitrogen in the dark in the freezer (below 8 Celsius)
儲存類別代碼
11 - Combustible Solids
水污染物質分類(WGK)
WGK 3
閃點(°F)
Not applicable
閃點(°C)
Not applicable