901655
Electroless nickel plating solution
ammonia free
Synonym(e):
Nickelex
About This Item
Empfohlene Produkte
Form
liquid
Farbe
blue to green
pH-Wert
4.8-5.2
Suchen Sie nach ähnlichen Produkten? Aufrufen Leitfaden zum Produktvergleich
Verwandte Kategorien
Allgemeine Beschreibung
Advantages
- Stable, ready to use
- Plates without generating ammonia fumes
- Produces quality electrical contacts on p- and n-type silicon
- Does not compensate for p- or n- type conductivity
- Excellent adhesion and solderability
- Plates on silicon, germanium, gallium arsenide, cadmium sulfide
The chemical reaction during the electroless plating process involves an oxidation-reduction reaction between nickelous and hypophosphite ions. The reaction is essentially a two step process occurring simultaneously.
(1) H2PO2- + H2O --> H2OPO3- + H2
(2) Ni ++ (complex) + H2 --> Ni + 2H+
The reaction progresses catalytically with nickel deposition occurring at the operating temperature of 95 °C - 100 °C. The nascent hydrogen evolved insures an oxide free nickel deposit. In addition some NiP formed in a side reaction improves corrosion resistance and solderability. The nickel deposit is highly conductive, remains unstressed, particularly after suitable heat treatment, and shows good adherence.
Anwendung
- Nickelex provides good mechanical and electrical contacts for semicodonductor devices (silicon rectifers, solar cells, varactors, microwave diodes, transistors, microcircuits, etc.). The quality of the electrical contact is excellent if the surface of silicon is abraded by lapping to increase surface recombination velocity; if the surface is highly doped from diffusion; or if the semicondcutor resistivity is low (0.1 ohm-cm). Nickelex also produces adherent deposits on germanium, gallium arsenide, and cadmium sulfide.
- The Nickelex plate exhibits excellent solderability with lead, tin, and Pb/Sn alloys. Flux can be omitted when furnaced soldered in a hydrogen or non-oxidizing atmosphere.
Instructions
Complete metallization procedures are provided for silicon rectifier and planar device fabrication. These procedures should be followed to obtain optimum adhesion of nickel and quality of the ohmic contacts.
Signalwort
Danger
Gefahreneinstufungen
Acute Tox. 3 Dermal - Acute Tox. 3 Oral - Acute Tox. 4 Inhalation - Aquatic Acute 1 - Aquatic Chronic 1 - Carc. 1A Inhalation - Eye Irrit. 2 - Muta. 2 - Repr. 1B - Resp. Sens. 1 - Skin Irrit. 2 - Skin Sens. 1 - STOT RE 1
Zielorgane
Lungs
Lagerklassenschlüssel
6.1C - Combustible, acute toxic Cat.3 / toxic compounds or compounds which causing chronic effects
WGK
WGK 3
Flammpunkt (°F)
Not applicable
Flammpunkt (°C)
Not applicable
Zulassungslistungen
Zulassungslistungen werden hauptsächlich für chemische Produkte erstellt. Für nicht-chemische Produkte können hier nur begrenzte Angaben gemacht werden. Kein Eintrag bedeutet, dass keine der Komponenten gelistet ist. Es liegt in der Verantwortung des Benutzers, die sichere und legale Verwendung des Produkts zu gewährleisten.
EU REACH Annex XVII (Restriction List)
Analysenzertifikate (COA)
Suchen Sie nach Analysenzertifikate (COA), indem Sie die Lot-/Chargennummer des Produkts eingeben. Lot- und Chargennummern sind auf dem Produktetikett hinter den Wörtern ‘Lot’ oder ‘Batch’ (Lot oder Charge) zu finden.
Besitzen Sie dieses Produkt bereits?
In der Dokumentenbibliothek finden Sie die Dokumentation zu den Produkten, die Sie kürzlich erworben haben.
Kunden haben sich ebenfalls angesehen
Unser Team von Wissenschaftlern verfügt über Erfahrung in allen Forschungsbereichen einschließlich Life Science, Materialwissenschaften, chemischer Synthese, Chromatographie, Analytik und vielen mehr..
Setzen Sie sich mit dem technischen Dienst in Verbindung.