901661
Zincate electroless immersion zinc plating solution
Autenticatiper visualizzare i prezzi riservati alla tua organizzazione & contrattuali
About This Item
Prodotti consigliati
Forma fisica
liquid
Colore
colorless to light yellow
pH
>10
Descrizione generale
Aluminum surfaces are not receptive to most plating processes due to their tendency to form oxides rapidly.Oxide formation inhibits uniform plating, resulting in inhomogeneous deposits, poor adhesion, or no deposition at all. By first applying Zincate Electroless Immersion Zinc Plating Solution to a properly prepared aluminum surface, it is possible subsequently deposit high quality electroless nickel films.
Applicazioni
Plating onto aluminum involves a multiple step process.
1.Non-etch clean the aluminum surface for up to 5 minutes with a detergent-based cleaner. Rinse thoroughly with cascading water.
2. De-smut the surface for 10-30 seconds using an acid mixture. RTM A for plastics is a suitable agent for smut removal. Rinse again thoroughly.
3. Mild etch for 5-10 seconds in a 25% solution of Aluminum Etch Type A. Rinse again thoroughly.
4. De-smut a second time and rinse as in step 2.
5. Apply the first Zincate layer. Immerse the part in the Zincate solution for 1-2 minutes at room temperature until a gray color develops. Rinse.
6. Remove the first Zincate layer using 50% nitric acid for 30-60 seconds or until the deposit turns white. Rinse.
7. Apply a second Zincate layer for 30-60 seconds. Rinse thoroughly before applying electroless nickel to the surface.
1.Non-etch clean the aluminum surface for up to 5 minutes with a detergent-based cleaner. Rinse thoroughly with cascading water.
2. De-smut the surface for 10-30 seconds using an acid mixture. RTM A for plastics is a suitable agent for smut removal. Rinse again thoroughly.
3. Mild etch for 5-10 seconds in a 25% solution of Aluminum Etch Type A. Rinse again thoroughly.
4. De-smut a second time and rinse as in step 2.
5. Apply the first Zincate layer. Immerse the part in the Zincate solution for 1-2 minutes at room temperature until a gray color develops. Rinse.
6. Remove the first Zincate layer using 50% nitric acid for 30-60 seconds or until the deposit turns white. Rinse.
7. Apply a second Zincate layer for 30-60 seconds. Rinse thoroughly before applying electroless nickel to the surface.
Avvertenze
Danger
Indicazioni di pericolo
Classi di pericolo
Aquatic Chronic 3 - Eye Dam. 1 - Met. Corr. 1 - Skin Corr. 1A
Codice della classe di stoccaggio
8B - Non-combustible corrosive hazardous materials
Classe di pericolosità dell'acqua (WGK)
WGK 1
Punto d’infiammabilità (°F)
Not applicable
Punto d’infiammabilità (°C)
Not applicable
Scegli una delle versioni più recenti:
Certificati d'analisi (COA)
Non trovi la versione di tuo interesse?
Se hai bisogno di una versione specifica, puoi cercare il certificato tramite il numero di lotto.
Possiedi già questo prodotto?
I documenti relativi ai prodotti acquistati recentemente sono disponibili nell’Archivio dei documenti.
Il team dei nostri ricercatori vanta grande esperienza in tutte le aree della ricerca quali Life Science, scienza dei materiali, sintesi chimica, cromatografia, discipline analitiche, ecc..
Contatta l'Assistenza Tecnica.