GF20493794

Tantalum

foil, 15mm disks, thickness 0.0125mm, 99.9%

Synonyme(s) :

Tantalum, TA000300, Ta

Se connecterpour consulter vos tarifs contractuels et ceux de votre entreprise/organisme


About This Item

Formule empirique (notation de Hill):
Ta
Numéro CAS:
Poids moléculaire :
180.95
Numéro MDL:
Code UNSPSC :
12141741
ID de substance PubChem :
Nomenclature NACRES :
NA.23

Le tarif et la disponibilité ne sont pas disponibles actuellement.

Pression de vapeur

<0.01 mmHg ( 537.2 °C)

Pureté

99.90%

Forme

foil

Température d'inflammation spontanée

572 °F

Fabricant/nom de marque

Goodfellow 204-937-94

Résistivité

13.5 μΩ-cm, 20°C

Diam. × épaisseur

15 mm × 0.0125 mm

Point d'ébullition

5425 °C (lit.)

Pf

2996 °C (lit.)

Densité

16.69 g/cm3 (lit.)

Description générale

For updated SDS information please visit www.goodfellow.com.

Informations légales

Product of Goodfellow

Faites votre choix parmi les versions les plus récentes :

Certificats d'analyse (COA)

Lot/Batch Number

Désolés, nous n'avons pas de COA pour ce produit disponible en ligne pour le moment.

Si vous avez besoin d'assistance, veuillez contacter Service Clients

Déjà en possession de ce produit ?

Retrouvez la documentation relative aux produits que vous avez récemment achetés dans la Bibliothèque de documents.

Consulter la Bibliothèque de documents

Yingxun Du et al.
Journal of hazardous materials, 225-226, 21-27 (2012-05-23)
In order to overcome the limitation of the application of nanoparticles, tantalum (oxy)nitrides nanotube arrays on a Ta foil were synthesized and introduced in vis (visible light)-Fenton-like system to enhance the degradation of atrazine. At first, the anodization of tantalum
Zhongli Cai et al.
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
J G Sen Gupta
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
Zhongli Cai et al.
Radiation research, 165(3), 365-371 (2006-02-24)
Both thick and thin films of pGEMR-3Zf- plasmid DNA deposited on a tantalum foil were exposed to soft X rays (effective energy of 14.8 keV) for various times in air under a relative humidity of 45% (Gamma approximately 6, where
J G Sen Gupta
Talanta, 32(1), 1-6 (1985-01-01)
An improved graphite furnace atomic-absorption method has been developed for the determination of Sc, Y and the rare-earth elements in silicate rocks and related materials. The method, which involves the separation of the lanthanides by ion-exchange followed by their determination

Notre équipe de scientifiques dispose d'une expérience dans tous les secteurs de la recherche, notamment en sciences de la vie, science des matériaux, synthèse chimique, chromatographie, analyse et dans de nombreux autres domaines..

Contacter notre Service technique