白石英砂

purum p.a., powder

同義詞:

二氧化硅, 石英

登入查看組織和合約定價


About This Item

線性公式:
SiO2
CAS號碼:
分子量::
60.08
EC號碼:
MDL號碼:
分類程式碼代碼:
12352300
PubChem物質ID:
NACRES:
NA.21

等級

purum p.a.

品質等級

形狀

powder

損耗

≤0.3% loss on ignition, 900 °C

粒徑

>230 mesh

負離子痕跡

chloride (Cl-): ≤50 mg/kg

正離子痕跡

Ca: ≤200 mg/kg
Cd: ≤50 mg/kg
Co: ≤50 mg/kg
Cu: ≤50 mg/kg
Fe: ≤200 mg/kg
K: ≤1000 mg/kg
Na: ≤150 mg/kg
Ni: ≤50 mg/kg
Pb: ≤100 mg/kg
Zn: ≤50 mg/kg

SMILES 字串

O=[Si]=O

InChI

1S/O2Si/c1-3-2

InChI 密鑰

VYPSYNLAJGMNEJ-UHFFFAOYSA-N

尋找類似的產品? 前往 產品比較指南

一般說明

本品为沙、白色石英(SiO2)。已有研究报道了它与碱性含有溶解的Al的NaNO3 溶液,在89℃下的反应。

應用

沙、白色石英(石英)已被用作固体样品,用于评估流体-岩石相互作用实验期间的孔体积变化。

分析報告

金属和氯化物痕迹是指酸溶性部分

象形圖

Health hazard

訊號詞

Danger

危險聲明

危險分類

STOT RE 1 Inhalation

標靶器官

Lungs

儲存類別代碼

6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects

水污染物質分類(WGK)

nwg

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析證明 (COA)

輸入產品批次/批號來搜索 分析證明 (COA)。在產品’s標籤上找到批次和批號,寫有 ‘Lot’或‘Batch’.。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

客戶也查看了

Pore-volume alteration measurements to evaluate scale formation during solid-fluid interactions.
Moola P, et al.
Mineralogical Magazine, 78(6), 1399-1403 (2014)
B R Bickmore et al.
Environmental science & technology, 35(22), 4481-4486 (2002-01-05)
Caustic NaNO3 solutions containing dissolved Al were reacted with quartz sand at 89 degrees C to simulate possible reactions between leaked nuclear waste and primary subsurface minerals at the U.S. Department of Energy's Hanford site in Washington. Nitrate-cancrinite began to
Mukesh K Jaiswal et al.
Journal of reproductive immunology, 112, 38-45 (2015-08-01)
The a2 isoform of vacuolar-ATPase (ATP6V0A2, referred to as a2V) is required for normal spermatogenesis and maturation of sperm. Treatment of male mice with anti-a2V disturbs the testicular cytokine/chemokine balance and leads to severe deficiencies of spermatogenesis. The aim of
Mukesh K Jaiswal et al.
Journal of leukocyte biology, 96(2), 337-347 (2014-03-14)
a2V is required for maturation of sperm. The decreased expression of a2V at the feto-maternal interphase causes poor pregnancy outcome. The present study examined the role of a2V in spermatogenesis and inflammatory network in the testis. A single dose of
G Cappelletti et al.
Environmental science and pollution research international, 22(22), 17733-17743 (2015-07-15)
In order to avoid both natural and artificial stone decay, mainly due to the interaction with atmospheric pollutants (both gases such as NOx and SO2 and particulate matter), polymeric materials have been widely studied as protective coatings enable to limit

我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.

聯絡技術服務