描述

Graphene oxide sheet size: 300-800 nm lateral size
Number of layer for graphene oxide: single layer

品質等級

形狀

liquid

特點

avg. no. of layers 1

環保替代產品特色

Design for Energy Efficiency
Learn more about the Principles of Green Chemistry.

sustainability

Greener Alternative Product

濃度

40 mg/mL (Graphene oxide aquous ink)

黏度

100-210 Pa.s (25 °C at shear rate of 10 s-1)

環保替代類別

儲存溫度

2-8°C

一般說明

We are committed to bringing you Greener Alternative Products, which adhere to one or more of The 12 Principles of Green Chemistry. This product has been enhanced for energy efficiency. Click here for more information.

應用

This product can be used in material extrusion 3D printing technique.
This product is a thixotropic ink based on graphene oxide (GO) nanosheets. It is suitable for various direct ink write (aka robocasting) printing technologies. The ink offers a stable dispersion of GO, high viscosity, good printability, and long shelf life. Freeze-dried and annealed patterns provide low electrical resistivity and high surface area. The ink is suitable for applications such as batteries, supercapacitors, electrocatalysis, etc.

準備報告

Before Printing:
Bring the ink to room temeprature, best to mix the ink in a planetary mixer before usage.

Printing:
Recommended 3D printing nozzle diameter size is 400 micron.

Post printing:
After 3D printing, this ink can be directly freeze-dried in liquid nitrogen and vacuum to obtain free- standing graphene oxide aerogel.
This ink can also be processed by adding gelling agents to enable a covalent bond established between the graphene oxide sheets. Gelation agents such as ammonium carbonate, ammonium hydroxide, resorcinol formaldehyde have all been reported to be sufficient. After gelation, the wet GO gels printed parts are washed in acetone to remove water from the pores. Supercritical CO2 can then be used to dry the GO gels.

Curing:
Parts that are printed with gelling agent can be cured in sealed glass vials at 85 °C.
The dried aerogels are generally reduced to graphene aerogels by thermal treatment at 1050 °C under inert atmosphere. Other chemical reduction methods include hydrazine reduction, dried aerogels can also be reduced using hydroiodic acid, followed by washing in ethanol, water and then freeze drying.

儲存和穩定性

Tighly seal remaining ink, and store in 2-8 °C fridge.

儲存類別代碼

10 - Combustible liquids

水污染物質分類(WGK)

WGK 3


從最近期的版本中選擇一個:

分析證明 (COA)

Lot/Batch Number

未看到正確版本?

如果您需要一個特定的版本,您可以透過批號來尋找特定憑證。

已經擁有該產品?

您可以在文件庫中找到最近購買的產品相關文件。

存取文件庫

Toward Macroscale, Isotropic Carbons with Graphene-Sheet-Like Electrical and Mechanical Properties.
Worsley M A, et al.
Advances in Functional Materials, 24(27), 4259-4264 (2014)
Versatile mechanically strong and highly conductive chemically converted graphene aerogels..
Liu Y, et al.
Carbon, 125, 352-359 (2017)
Bin Yao et al.
Advanced materials (Deerfield Beach, Fla.), 32(8), e1906652-e1906652 (2020-01-18)