推薦產品
化驗
≥99.99% trace metals basis
形狀
flakes
電阻係數
9.71 μΩ-cm
直徑× 厚度
<25 mm × 4-6 mm
bp
2750 °C (lit.)
mp
1535 °C (lit.)
密度
7.86 g/mL at 25 °C (lit.)
SMILES 字串
[Fe]
InChI
1S/Fe
InChI 密鑰
XEEYBQQBJWHFJM-UHFFFAOYSA-N
儲存類別代碼
4.1B - Flammable solid hazardous materials
水污染物質分類(WGK)
nwg
閃點(°F)
Not applicable
閃點(°C)
Not applicable
客戶也查看了
文章
An article concerning self-propagating reactions induced by mechanical alloying, presented by Sigma-Aldrich.com.
In recent years, the price of tellurium, a key component in the bestperforming thermoelectric materials, has increased significantly, leading to the question, “Is it economically viable to produce thermoelectric generators on an industrial scale?
The price of tellurium, a key component in many thermoelectric materials, has risen in recent years, leading to the search for more cost-effective substitutes. This article presents silicide materials as a cheaper potential alternative.
我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.
聯絡技術服務