Polyethylene

Ultra-high molecular weight, average Mw 3,000,000-6,000,000

Synonym(s):

PE

Sign Into View Organizational & Contract Pricing


About This Item

Linear Formula:
H(CH2CH2)nH
CAS Number:
MDL number:
UNSPSC Code:
12162002
PubChem Substance ID:
NACRES:
NA.23

description

coefficient of friction: 0.20 - 0.25

(Cr-plated steel, 23°C, static, ASTM D 1894)

form

powder

mol wt

average Mw 3,000,000-6,000,000

hardness

52 (Rockwell R, ASTM D 785)

transition temp

softening point 136 °C (Vicat, ASTM D 1525B)
Tm 138 °C (DSC)

density

0.94 g/mL at 25 °C

InChI

1S/C2H4/c1-2/h1-2H2

InChI key

VGGSQFUCUMXWEO-UHFFFAOYSA-N

Looking for similar products? Visit Product Comparison Guide

Application

Bearings, gears, bushings and other moving parts.

Features and Benefits

Self-lubricating extraordinary wear properties.
Abrasion, corrosion and impact resistance exceeds many conventional materials, including steel and expensive metals and alloys.

Storage Class Code

11 - Combustible Solids

WGK

WGK 3

Personal Protective Equipment

dust mask type N95 (US), Eyeshields, Gloves

Choose from one of the most recent versions:

Certificates of Analysis (COA)

Lot/Batch Number

Don't see the Right Version?

If you require a particular version, you can look up a specific certificate by the Lot or Batch number.

Already Own This Product?

Find documentation for the products that you have recently purchased in the Document Library.

Visit the Document Library

Eliandra Mirlei Rossi et al.
Journal of infection in developing countries, 7(3), 229-234 (2013-03-16)
Contaminated sponges might lead to cross-contamination in kitchens since they can transfer microorganisms to surfaces where microorganisms can survive for hours or days and contaminate food. The main objective of this study was to evaluate the transfer and the survival
Morteza Meftah et al.
The Journal of bone and joint surgery. American volume, 95(13), 1193-1197 (2013-07-05)
Ceramic femoral heads produce less wear of the opposing polyethylene than do metal femoral heads in wear simulation studies. This is a matched-pair analysis of the wear of ceramic and metal femoral heads on conventional polyethylene in uncemented total hip
Ingvild Bostadløkken et al.
Ugeskrift for laeger, 175(13), 891-892 (2013-04-16)
We present a case of a 66-year-old woman who had a total knee arthroplasty. Shortly after surgery a 90° rotation of her polyethylene liner took place. The complication was undiagnosed for 1.5 years. To know this problem and be able
Alicia E Leadford et al.
Pediatrics, 132(1), e128-e134 (2013-06-05)
Hypothermia contributes to neonatal mortality and morbidity, especially in preterm and low birth weight infants in developing countries. Plastic bags covering the trunk and extremities of very low birth weight infants reduces hypothermia. This technique has not been studied in
Kelly M Seymour et al.
Journal of biomechanical engineering, 135(2), 021017-021017 (2013-03-01)
Ultra high molecular weight polyethylene (UHMWPE, or ultra high), a frequently used material in orthopedic joint replacements, is often the cause of joint failure due to wear, fatigue, or fracture. These mechanical failures have been related to ultra high's strength

Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.

Contact Technical Service