GF07210347

foil, 10m coil, thickness 0.025mm, coil width 0.75mm, annealed, 99.9%

别名:

钽, Ta

登录查看公司和协议定价


About This Item

经验公式(希尔记法):
Ta
CAS号:
分子量:
180.95
MDL號碼:
分類程式碼代碼:
12141741
PubChem物質ID:
NACRES:
NA.23

蒸汽壓力

<0.01 mmHg ( 537.2 °C)

化驗

99.9%

形狀

foil

自燃溫度

572 °F

製造商/商標名

Goodfellow 072-103-47

電阻係數

13.5 μΩ-cm, 20°C

長度 × 厚度 × 寬度

10 m × 0.025 mm × 0.75 mm

bp

5425 °C (lit.)

mp

2996 °C (lit.)

密度

16.69 g/cm3 (lit.)

SMILES 字串

[Ta]

InChI

1S/Ta

InChI 密鑰

GUVRBAGPIYLISA-UHFFFAOYSA-N

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

从最新的版本中选择一种:

分析证书(COA)

Lot/Batch Number

抱歉,我们目前尚未线上提供该产品的COA。

如需帮助,请联系 客户支持

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

Yingxun Du et al.
Journal of hazardous materials, 225-226, 21-27 (2012-05-23)
In order to overcome the limitation of the application of nanoparticles, tantalum (oxy)nitrides nanotube arrays on a Ta foil were synthesized and introduced in vis (visible light)-Fenton-like system to enhance the degradation of atrazine. At first, the anodization of tantalum
Zhongli Cai et al.
The journal of physical chemistry. B, 109(10), 4796-4800 (2006-07-21)
Both monolayer and thick (20 microm) films of dry pGEM-3Zf(-) plasmid DNA deposited on tantalum foil were exposed to Al Kalpha X-rays (1.5 keV) for various times in an ultrahigh vacuum chamber. For monolayer DNA, the damage was induced mainly
J G Sen Gupta
Talanta, 31(12), 1053-1056 (1984-12-01)
A 40-fold increase in sensitivity obtained by using a tantalum foil lining in a pyrolytically-coated graphite furnace permitted determination of low ppm levels of cerium in most silicate rocks. A preliminary preconcentration by oxalate and hydroxide co-precipitations was used before
Zhongli Cai et al.
Radiation research, 165(3), 365-371 (2006-02-24)
Both thick and thin films of pGEMR-3Zf- plasmid DNA deposited on a tantalum foil were exposed to soft X rays (effective energy of 14.8 keV) for various times in air under a relative humidity of 45% (Gamma approximately 6, where
J G Sen Gupta
Talanta, 32(1), 1-6 (1985-01-01)
An improved graphite furnace atomic-absorption method has been developed for the determination of Sc, Y and the rare-earth elements in silicate rocks and related materials. The method, which involves the separation of the lanthanides by ion-exchange followed by their determination

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门