GF40266682

Sigma-Aldrich

Lithium

foil, not light tested, 38x500mm, thickness 0.20mm, as rolled, 99.9%

동의어(들):

Lithium, LI000220

로그인조직 및 계약 가격 보기


About This Item

Linear Formula:
Li
CAS Number:
Molecular Weight:
6.94
MDL number:
UNSPSC 코드:
12141803
PubChem Substance ID:
NACRES:
NA.23

분석

99.9%

형태

foil

제조업체/상표

Goodfellow 402-666-82

저항도

9.446 μΩ-cm, 20°C

크기 × 두께

38x500 mm × 0.20 mm

bp

1342 °C (lit.)

mp

180 °C (lit.)

density

0.534 g/mL at 25 °C (lit.)

SMILES string

[Li]

InChI

1S/Li

InChI key

WHXSMMKQMYFTQS-UHFFFAOYSA-N

유사한 제품을 찾으십니까? 방문 제품 비교 안내

일반 설명

For updated SDS information please visit www.goodfellow.com.

애플리케이션

  • A retrospective on lithium-ion batteries: This article reviews the contributions in the development of lithium-ion batteries, discussing inspirational insights to guide future breakthroughs in battery technology (J Xie, YC Lu, 2020).
  • Guidelines and trends for next-generation rechargeable lithium and lithium-ion batteries: This review discusses the limitations of commercial lithium-ion batteries and explores the directions for next-generation batteries (F Wu, J Maier, Y Yu, 2020).
  • Prospects for lithium-ion batteries and beyond—a 2030 vision: This article explores the future of lithium-ion batteries and discusses current strategies to improve these and next-generation battery technologies (CP Grey, DS Hall, 2020).
  • Lithium brines: A global perspective: This study offers a global perspective on lithium brines, discussing the critical and technologically important roles of lithium, which is in increasing demand (LA Munk, SA Hynek, DC Bradley, D Boutt, K Labay, 2016).

법적 정보

Product of Goodfellow

Storage Class Code

4.3 - Hazardous materials which set free flammable gases upon contact with water

WGK

WGK 1

Flash Point (°F)

Not applicable

Flash Point (°C)

Not applicable


가장 최신 버전 중 하나를 선택하세요:

시험 성적서(COA)

Lot/Batch Number

죄송합니다. 지금은 이 제품에 대한 COA이(가) 온라인에서 제공되지 않습니다.

도움이 필요하시면 연락하세요. 고객 지원 부서

이 제품을 이미 가지고 계십니까?

문서 라이브러리에서 최근에 구매한 제품에 대한 문서를 찾아보세요.

문서 라이브러리 방문

Xianglong Li et al.
Nanoscale, 5(19), 8864-8873 (2013-08-15)
The implementation of silicon (Si) in practical lithium ion battery electrodes has been hindered due to its large volume change and consequent structural and interfacial instabilities. Coating nanostructured Si with a second phase (e.g., carbon (C)) represents a very promising
Rebecca F McKnight et al.
Lancet (London, England), 379(9817), 721-728 (2012-01-24)
Lithium is a widely used and effective treatment for mood disorders. There has been concern about its safety but no adequate synthesis of the evidence for adverse effects. We aimed to undertake a clinically informative, systematic toxicity profile of lithium.
Susan W Lehmann et al.
Journal of affective disorders, 146(2), 151-157 (2012-09-19)
Lithium has been reported to induce hypercalcemia and hyperparathyroidism, yet few studies have examined the impact on older patients. We therefore undertook this review and report our findings. We undertook a systematic review of articles on lithium-associated hypercalcemia and/or hyperparathyroidism
Annemiek Dols et al.
International clinical psychopharmacology, 28(6), 287-296 (2013-07-23)
Side effects are among the most frequent reasons preventing patients from taking their medication. Although the management of side effects is an important issue in clinical practice, particularly in patients with physical comorbidities, research on clinical management of side effects
Yingying Lu et al.
Nature materials, 13(10), 961-969 (2014-08-12)
Rechargeable lithium, sodium and aluminium metal-based batteries are among the most versatile platforms for high-energy, cost-effective electrochemical energy storage. Non-uniform metal deposition and dendrite formation on the negative electrode during repeated cycles of charge and discharge are major hurdles to

자사의 과학자팀은 생명 과학, 재료 과학, 화학 합성, 크로마토그래피, 분석 및 기타 많은 영역을 포함한 모든 과학 분야에 경험이 있습니다..

고객지원팀으로 연락바랍니다.