descripción

coefficient of friction: 0.20 - 0.25

(Cr-plated steel, 23°C, static, ASTM D 1894)

Nivel de calidad

formulario

powder

mol peso

average Mw 3,000,000-6,000,000

dureza

52 (Rockwell R, ASTM D 785)

temperatura de transición

softening point 136 °C (Vicat, ASTM D 1525B)
Tm 138 °C (DSC)

densidad

0.94 g/mL at 25 °C

InChI

1S/C2H4/c1-2/h1-2H2

Clave InChI

VGGSQFUCUMXWEO-UHFFFAOYSA-N

¿Está buscando productos similares? Visita Guía de comparación de productos

Aplicación

Bearings, gears, bushings and other moving parts.

Características y beneficios

Self-lubricating extraordinary wear properties.
Abrasion, corrosion and impact resistance exceeds many conventional materials, including steel and expensive metals and alloys.

Código de clase de almacenamiento

11 - Combustible Solids

Clase de riesgo para el agua (WGK)

WGK 3

Equipo de protección personal

Eyeshields, Gloves, type N95 (US)


Elija entre una de las versiones más recientes:

Certificados de análisis (COA)

Lot/Batch Number

¿No ve la versión correcta?

Si necesita una versión concreta, puede buscar un certificado específico por el número de lote.

¿Ya tiene este producto?

Encuentre la documentación para los productos que ha comprado recientemente en la Biblioteca de documentos.

Visite la Librería de documentos

Los clientes también vieron

Eliandra Mirlei Rossi et al.
Journal of infection in developing countries, 7(3), 229-234 (2013-03-16)
Contaminated sponges might lead to cross-contamination in kitchens since they can transfer microorganisms to surfaces where microorganisms can survive for hours or days and contaminate food. The main objective of this study was to evaluate the transfer and the survival
Morteza Meftah et al.
The Journal of bone and joint surgery. American volume, 95(13), 1193-1197 (2013-07-05)
Ceramic femoral heads produce less wear of the opposing polyethylene than do metal femoral heads in wear simulation studies. This is a matched-pair analysis of the wear of ceramic and metal femoral heads on conventional polyethylene in uncemented total hip
Ingvild Bostadløkken et al.
Ugeskrift for laeger, 175(13), 891-892 (2013-04-16)
We present a case of a 66-year-old woman who had a total knee arthroplasty. Shortly after surgery a 90° rotation of her polyethylene liner took place. The complication was undiagnosed for 1.5 years. To know this problem and be able
Alicia E Leadford et al.
Pediatrics, 132(1), e128-e134 (2013-06-05)
Hypothermia contributes to neonatal mortality and morbidity, especially in preterm and low birth weight infants in developing countries. Plastic bags covering the trunk and extremities of very low birth weight infants reduces hypothermia. This technique has not been studied in
Kelly M Seymour et al.
Journal of biomechanical engineering, 135(2), 021017-021017 (2013-03-01)
Ultra high molecular weight polyethylene (UHMWPE, or ultra high), a frequently used material in orthopedic joint replacements, is often the cause of joint failure due to wear, fatigue, or fracture. These mechanical failures have been related to ultra high's strength

Nuestro equipo de científicos tiene experiencia en todas las áreas de investigación: Ciencias de la vida, Ciencia de los materiales, Síntesis química, Cromatografía, Analítica y muchas otras.

Póngase en contacto con el Servicio técnico