Polypropylene, isotactic
average Mw ~250,000 by GPC
Sign Into View Organizational & Contract Pricing
All Photos(2)
About This Item
Recommended Products
form
solid
autoignition temp.
>674 °F
mol wt
average Mw ~250,000 by GPC
refractive index
n20/D 1.49 (lit.)
mp
189 °C (lit.)
transition temp
Tg −26 °C
density
0.9 g/mL at 25 °C (lit.)
Related Categories
Storage Class Code
11 - Combustible Solids
WGK
WGK 3
Flash Point(F)
Not applicable
Flash Point(C)
Not applicable
Personal Protective Equipment
dust mask type N95 (US), Eyeshields, Gloves
Choose from one of the most recent versions:
Already Own This Product?
Find documentation for the products that you have recently purchased in the Document Library.
Customers Also Viewed
Polymers, 11(2) (2019-04-10)
Strain hardening has important roles in understanding material structures and polymer processing methods, such as foaming, film forming, and fiber extruding. A common method to improve strain hardening behavior is to chemically branch polymer structures, which is costly, thus preventing
Our team of scientists has experience in all areas of research including Life Science, Material Science, Chemical Synthesis, Chromatography, Analytical and many others.
Contact Technical Service