推薦產品
材料
off-white silicone body (123 mil thick)
yellow PTFE face (2 mil thick)
包裝
pkg of 100 ea
直徑
9.5 mm ( 3/8 in.)
尋找類似的產品? 前往 產品比較指南
一般說明
PTFE-faced septa are suitable to overcome the degradation due to prolonged high temperatures which occurs in silicone rubber septa. The degradation results in baseline drift and additional peaks. It is generally fixed with the PTFE faced towards the column packing.
PTFE面隔垫专门用于需要更大惰性的应用。类白色硅胶体(123 mil厚)为黄色PTFE面(2 mil厚)提供了大量支撑。注射时PTFE破裂后,可能会发生一些流血。由于这种出血随着橡胶暴露而增加,因此我们建议使用针头引导来减小穿刺区域的大小。在200℃至300℃的入口温度下使用。
應用
Glass vials equipped with stir bars may be sealed with PTFE faced silicone septa for solvent drop microextraction analysis of water samples. This may be used in sealing the vials used for headspace solid-phase microextraction (HS-SPME) procedure during determination of aldehydes in drinking water.
Journal of chromatography. A, 943(1), 1-13 (2002-02-01)
A headspace solid-phase microextraction (HS-SPME) procedure followed by gas chromatography and electron capture detection (GC-ECD) has been developed for the determination of aldehydes in drinking water samples at microg/l concentrations. A previous derivatization with o-(2,3,4,5,6-pentafluorobenzyl)hydroxylamine hydrochloride (PFBHA) was performed due
Analytical and bioanalytical chemistry, 383(4), 557-561 (2005-09-01)
Water contamination due to the wide variety of pesticides used in agriculture practices is a global environmental pollution problem. Analytical methods with low quantification limits are necessary. The application of a new extraction technique, solvent drop microextraction (SDME), followed by
Gas Chromatography, 62-62 (2008)
我們的科學家團隊在所有研究領域都有豐富的經驗,包括生命科學、材料科學、化學合成、色譜、分析等.
聯絡技術服務