跳转至内容
Merck

GF27664836

foil, 4mm disks, thickness 0.008mm, 99.95%

别名:

登录查看公司和协议定价


About This Item

经验公式(希尔记法):
Ni
CAS号:
分子量:
58.69
MDL號碼:
分類程式碼代碼:
12141729
PubChem物質ID:
NACRES:
NA.23

化驗

99.95%

形狀

foil

製造商/商標名

Goodfellow 276-648-36

電阻係數

6.97 μΩ-cm, 20°C

直徑× 厚度

4 mm × 0.008 mm

bp

2732 °C (lit.)

mp

1453 °C (lit.)

密度

8.9 g/mL at 25 °C (lit.)

SMILES 字串

[Ni]

InChI

1S/Ni

InChI 密鑰

PXHVJJICTQNCMI-UHFFFAOYSA-N

一般說明

For updated SDS information please visit www.goodfellow.com.

法律資訊

Product of Goodfellow

象形圖

Health hazardExclamation mark

訊號詞

Danger

危險聲明

危險分類

Carc. 2 - Skin Sens. 1 - STOT RE 1

儲存類別代碼

6.1D - Non-combustible acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects

水污染物質分類(WGK)

WGK 1

閃點(°F)

Not applicable

閃點(°C)

Not applicable


分析证书(COA)

输入产品批号来搜索 分析证书(COA) 。批号可以在产品标签上"批“ (Lot或Batch)字后找到。

已有该产品?

在文件库中查找您最近购买产品的文档。

访问文档库

R J Schulz et al.
Physics in medicine and biology, 35(11), 1563-1574 (1990-11-01)
The thermal defects of A-150 plastic and graphite referenced to aluminium were determined for 800 keV protons scattered by a 2 micron nickel foil (mean transmitted energy = 550 keV). Composite cores of Al/A-150, graphite/A-150 and Al/graphite which could be
Kwanghyun Yoo et al.
Nanotechnology, 24(20), 205302-205302 (2013-04-20)
We firstly introduce a facile method for the site-specific direct physical exfoliation of few-layer graphene sheets from cheap and easily enlargeable graphite grown on a Ni foil using an optimized polydimethylsiloxane (PDMS) stamp. By decreasing the PDMS cross-linking time, the
G E van Dorssen et al.
Journal of X-ray science and technology, 3(2), 109-117 (1992-01-01)
The structure of Ni-C multilayer and single nickel layer samples has been analyzed before and after annealing, using two techniques: fluorescence EXAFS (F1EXAFS) at the Ni-K. edge and CuKα reflection. Annealing at a temperature of 450°C resulted in a change
F E Cecil et al.
The Review of scientific instruments, 81(10), 10D326-10D326 (2010-11-09)
We have examined the observed currents in the front foils of the JET Faraday cup lost alpha particle diagnostic KA-2. In particular, we have sought to understand the currents during Ohmic plasmas for which the ion flux at the detectors
W K Winnett et al.
Talanta, 41(10), 1627-1630 (1994-10-01)
A modification of the sample introduction system for combustion total organic carbon analyzers is presented where sample is sprayed into the instrument. Thermally created sprays and nebulizer sprays are discussed. It is shown that spray introduction gives more symmetric signals

我们的科学家团队拥有各种研究领域经验,包括生命科学、材料科学、化学合成、色谱、分析及许多其他领域.

联系技术服务部门