Catalyst Screening followed by TLC-MS for Reaction Progress Analysis using KitAlysis™
Sarah Trice, Thorsten vom Stein, Michael Schulz
Introduction
Catalyst screening is an important prerequisite in organic synthesis. KitAlysis™ High-Throughput Screening Kits showcase the most widely used catalytic methods of synthetic chemists, translated into an off-the-shelf screening system to quickly and efficiently identify or optimize suitable catalytic reaction conditions.
To evaluate the screening an analysis tool is needed. Thin layer chromatography (TLC) allows for a fast and cost-effective determination of the reaction progress by parallel analysis of the samples on one plate. This setup perfectly fits to the parallel synthesis utilizing KitAlysis™.
This application note displays the use of the KitAlysis™ High-Throughput Buchwald-Hartwig Amination Reaction Screening Kit for the optimization of the coupling of aryl bromide and diphenylamine combined with an evaluation of the result with TLC-MS analysis.
![Schematic reaction showing the coupling of aryl bromide (1) and diphenylamine (2) to form biphenyl-4-yl-di-p-tolyl-amine (3) Schematic reaction showing the coupling of aryl bromide (1) and diphenylamine (2) to form biphenyl-4-yl-di-p-tolyl-amine (3), where the product has a molecular weight of 349.468 g/Mol.](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/arylbromide/arylbromide.jpg)
Figure 1.Schematic reaction showing the coupling of aryl bromide (1) and diphenylamine (2) to form biphenyl-4-yl-di-p-tolyl-amine (3), where the product has a molecular weight of 349.468 g/Mol.
Results and Discussion
The two reactants, aryl bromide and diphenylamine, were applied in addition to the samples. The samples were clearly visible under UV-light, therefore no derivatization was necessary. Figures 2a, 2b and 2c show the developed plate under white light, at 254 nm and at 366 nm.
![Developed plate under white light Developed plate under white light](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/developed-plate-a/developed-plate-a.jpg)
Figure 2a.Developed plate under white light
![Developed plate at 254 nm Developed plate at 254 nm](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/developed-plate-b/developed-plate-b.jpg)
Figure 2b.Developed plate at 254 nm
![Developed plate at 366 nm Developed plate at 366 nm](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/developed-plate-c/developed-plate-c.jpg)
Figure 2c.Developed plate at 366 nm
Confirmation of reaction product by mass spectrometry: Formation of ACN adduct via radical ionization
![Mass spectrum (ESI+) of product [M+ACN] Mass spectrum (ESI+) of product [M+ACN]](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/mass-spectrum/mass-spectrum.jpg)
Figure 3.Mass spectrum (ESI+) of product [M+ACN]
![Biphenyl-4-yl-di-p-tolyl-amine Biphenyl-4-yl-di-p-tolyl-amine (M=349.568 g/Mol)](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/biphenyl/biphenyl.jpg)
Biphenyl-4-yl-di-p-tolyl-amine (M=349.568 g/Mol)
![KitAnalysis KitAlysis™](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/kitalysis/kitalysis.jpg)
![KitAnalysis products KitAlysis™](/deepweb/assets/sigmaaldrich/marketing/global/images/technical-documents/protocols/analytical-chemistry/thin-layer-chromatography/catalyst-screening-followed-by-tlc-ms/kitalysis2/kitalysis2.jpg)
To continue reading please sign in or create an account.
Don't Have An Account?